Typical Mechanical Properties
AISI # Tensile (KSI) Yield (KSI) % Elongation 2" Gage Reduction of Area
75K-1045V 90 75 14 25
100K – 1045/1050 115 100 8 20

** Tensile and Yield strength will vary with diameter of the bar

75,000 Min Yield       C1045 Micro Alloyed Cold Finished Bar
100,000 Min Yield     C1045/1050 Cold Drawn, Stress Relieved, A311-B

Typical Chemical Composition
C Mn P S Si Ni Cr Mo Cu Sn Al V
0.460 0.870 0.008 0.026 0.270 0.090 0.110 0.029 0.280 0.009 0.006 0.093
Standard Plating Specifications
Chrome thickness: 0.0005" minimum
Chrome hardness: 68/70 Rockwell C
Surface finish: 6-12 uin Ra
Salt Spray: 120 hours per ASTM B-117
Tolerance After Plating
1.00" to 2.50" Dia: + 0.0000 / – 0.0015
2.75" to 3.00" Dia: + 0.0000 / – 0.0020
3.25" to 4.00" Dia: + 0.0000 / – 0.0030
Precise Hard Chrome